An amorphous C68Fe24Zr8(3 onm)/Al70Zr30(3 nm)/Co68Fe24Zr8(3 nm) trilayer system has been
investigated using in-plane and out-of-plane angular dependent ferromagnetic resonance at
different frequencies. The in-plane magnetic anisotropy is uniaxial, retaining its value of
(2.960.1)103 J/m3 for each magnetic layer, whereas its direction was tailored independently in
an arbitrary manner by applying an external magnetic field during the film deposition. The
perpendicular anisotropy constant, supposed to reflect the interface quality, is nearly identical for
both layers. Furthermore, the magnetic layers act independently upon each other due to the absence
of interlayer coupling